Department Microstructure and Residual Stress Analysis
Setup Specs
Instrument | E3 | ||
Take off angle of monochromator [°] | 65 | ||
Wavelength [nm] | 0.147 | ||
Collimation [’] | open | ||
FWHM standard powder [°] | ~0.3 (at 2theta = 70°) | ||
Flux [n/cm2/s] | ~5 x 106 | ||
Detector | PSD 30 x 30 cm² | ||
Monochromator | Si (400), Double Focussing |