Institut Silizium-Photovoltaik
Charge separation in the bulk and at interfaces with metal halide perovskites
Properties such as the diffusion length and carrier lifetimes of metal halide perovskites depend on the preparation conditions, morphology, stoichiometry and the formation of intermediate phases [1,2]. Our institute provide tools for measuring diffusion length by Goodman method [1].
references
[1] Diffusion length of photo-generated charge carriers in layers and powders of CH3NH3PbI3 perovskite; Dittrich, T.; Lang, F.; Shargaieva, O.; Rappich, J.; Nickel, N.H.; Unger, E.; Rech, B.; Applied Physics Letters 109 (2016) 073901