Öffnet in neuem Fenster Opens in a new window Öffnet externe Seite Opens an external site Öffnet externe Seite in neuem Fenster Opens an external site in a new window

Abteilung Mikrostruktur- und Eigenspannungsanalyse

Die folgenden Inhalte sind nur in Englisch verfügbar

Sample environment

The E3 is capable to use environment such as furnaces and cryostats provided and services by the HZB sample environment group. If you plan to use such devices for your measurement, mention that in your beamtime proposal and/or contact us. However, further devices can exclusively be used on E3 to measure your samples.

Sample table / mounting

Detailed dimensions of the sample plates are provided via the download box.


Goniometer

We further provide an open goniometer tilt stage to mount samples of up to 50 kg and measure three perpendicular strain directions consecutively with one alignment. Optionally, another rotation stage on top of the goniometer can be used to measure extra orientations or let the sample continuously rotate in order to increase grain statistics, for example. Figure 2 demonstrates this setup.

vergrößerte Ansicht

Fig. 2: The goniometer table enables measurements of multiple sample orientations within one setup.


Load frame (tension/compression)

    vergrößerte Ansicht

    Fig. 1: Tiltable load frame.

    Since 2013, a new load frame for tension and compression tests of up to 50 kN load capacity is available on E3. The machine is mounted on a tiltable stage to have access to three perpendicular sample orientations within one alignment[1]. Figure 5 demonstrates this capability. Although, the device’s load cell and the available extensometer are controlled by a proprietary measuring and controlling system an interface has been created to use the load frame with the E3 instrument control software CARESS, such that scans against loads and strains are possible.

    Various sample grips allow testing samples of different shapes and sizes as shown in figure 6. If you plan to use the load frame during your beamtime, contact us to discuss your sample geometry. Detailed sample holder information is provided by the download box.

    vergrößerte Ansicht

    Fig. 2: Click picture to watch the frame tilting.

    vergrößerte Ansicht

    Fig. 3: Available sample grips for the loadframe. To indicate the different geometries the samples are highlighted in red.


    Additionally, a shared load frame to also allow for torsion tests is available in collaboration with the HZB neutron radiography& tomography and the University of Tennessee Knoxville (UTK)[2].

    References:

    [1] Rotatable multifunctional load frames for neutron diffractometers at FRM II - design, specifications and applications, M. Hoelzel et. al. (2013), Nucl. Instrum. Methods Phys. Res., Sect. A 711, 101-105, doi: 10.1016/j.nima.2013.01.049

    [2] Neutron Bragg-edge-imaging for strain mapping under in situ tensile loading, R. Woraceket. al. (2011), J. Appl. Phys. 109(9), 093506, doi: 10.1063/1.3582138